Nickel Alloy, Corrosion and Heat-Resistant, Wire 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Solution Heat Treated, Precipitation Hardenable. Original standard SAE AMS5699H-2022 in PDF full version. Additional info + preview on request
Document status: Active
Steel, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Forging Stock 13.5Cr - 13.5Ni - 0.35Mo - 2.2W Annealed. Original standard SAE AMS5700H-2022 in PDF full version. Additional info + preview on request
Document status: Active
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Flash Welded Rings and Forging Stock 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode Remelted or Vacuum Induction Melted 1800 °F (982 °C) Solution Heat Treated. Original standard SAE AMS5701G-2023 in PDF full version. Additional info + preview on request
Document status: Active
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings and Stock for Forging 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode Remelted or Vacuum Induction Melted 1750 °F (954 °C) Solution Heat Treated. Original standard SAE AMS5702F-2023 in PDF full version. Additional info + preview on request
Document status: Active
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings and Stock for Forging 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750 °F (954 °C) Solution, Stabilization, and Precipitation Heat Treated. Original standard SAE AMS5703F-2023 in PDF full version. Additional info + preview on request
Document status: Active
Nickel Alloy, Corrosion and Heat Resistant, Forgings 57Ni - 19.5Cr - 13.5Co - 4.6Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated. Original standard SAE AMS5704L-2020 in PDF full version. Additional info + preview on request
Document status: Active