Steel, Bars and Forgings, Nitriding 1.6Cr - 0.35Mo - 1.1Al (0.38 - 0.43C) (135 Mod) Hardened and Tempered, 112 ksi (772 MPa) Tensile Strength. Original standard SAE AMS 6472F-2014 in PDF full version. Additional info + preview on request
Document status: Replaced by
Steel, Bars and Forgings, Nitriding 1.6Cr - 0.35Mo - 1.1Al (0.38 - 0.43C) (135 Mod) Hardened and Tempered, 112 ksi (772 MPa) Tensile Strength. Original standard SAE AMS 6472G-2018 in PDF full version. Additional info + preview on request
Document status: Replaced by
Steel, Bars, Forgings, and Tubing 1.45Cr (0.93-1.05C) (SAE 52100) Special Aircraft-Quality Cleanliness. Original standard SAE AMS 6479D-2015 in PDF full version. Additional info + preview on request
Document status: Replaced by
Steel, Bars, Wire, and Forgings 8V - 4Cr - 4W - 3Mo (2.45 - 2.55C) Powder Metallurgy Product Hot Isostatically Pressed. Original standard SAE AMS 6556-2013 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS6556A-2023
Steel, Bars, Wire, and Forgings 9V - 5.25Cr - 1.3Mo (1.80 - 1.95C) Powder Metallurgy Product Hot Isostatically Pressed. Original standard SAE AMS 6557-2013 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS6557A-2023
Steel, Bars, Wire, and Forgings 10.5 Mo - 6 W - 3.75 Cr - 2 V (1.25 - 1.40 C) Powder Metallurgy Product Hot Isostatically Pressed. Original standard SAE AMS 6558-2013 in PDF full version. Additional info + preview on request