Turkmenistan standards PDF

↑
St SAE AMS 5316D-2013

Ductile (Nodular) Iron Castings, Sand 80,000 psi (550 MPa) Tensile Strength As Cast. Original standard SAE AMS 5316D-2013 in PDF full version. Additional info + preview on request

Document status: Replaced by St SAE AMS5316E-2017

€35
St SAE AMS 5333G-2017

Steel, Investment Castings 0.50Cr - 0.55Ni - 0.25Mo (0.11 - 0.17C) (SAE 8615) Normalized. Original standard SAE AMS 5333G-2017 in PDF full version. Additional info + preview on request

Document status: Active

€35
St SAE AMS 5334J-2018

Steel, Investment Castings 0.50Cr - 0.55Ni - 0.20Mo (0.25 - 0.35C) (SAE 8630 Mod) Normalized and Tempered. Original standard SAE AMS 5334J-2018 in PDF full version. Additional info + preview on request

Document status: Active

€35
St SAE AMS 5336J-2017

Steel, Investment Castings 0.95Cr - 0.20Mo (0.25 - 0.35C) (4130 Mod) Normalized or Normalized and Tempered. Original standard SAE AMS 5336J-2017 in PDF full version. Additional info + preview on request

Document status: Active

€35
St SAE AMS 5337E-2017

Steel, Maraging, Investment Castings 18.5Ni - 9.0Co - 5.0Mo - 0.70Ti - 0.12Al Vacuum Melted Homogenized, Overaged, and Solution Heat Treated. Original standard SAE AMS 5337E-2017 in PDF full version. Additional info + preview on request

Document status: Active

€35
St SAE AMS 5338H-2017

Steel, Investment Castings 0.95Cr - 0.20Mo (0.35 - 0.45C) (4140 Mod) Normalized or Normalized and Tempered. Original standard SAE AMS 5338H-2017 in PDF full version. Additional info + preview on request

Document status: Active

€35
↑